PRODUCT INFOMATION
The finished product technical specifications comply with the requirements outlined in ASTM C348, ASTM C349, ASTM C940.
The typical data are shown in the table below:
|
No. |
Item |
Performance Index |
||
|
1 |
Initial fluidity(20°C)/mm |
≥290 |
||
|
2 |
30 minutes fluidity(20°C)/mm |
≥260 |
||
|
3 |
Reaction temperature/°C |
Normal temperature |
||
|
4 |
Expansion ratio |
0.1%-2% |
||
|
5 |
Water-cement ratio |
0.12-0.14 |
||
|
6 |
Bleeding rate/% |
0 |
||
|
7 |
28-day dry shrinkage/% |
≤0.045 |
||
|
8 |
Effect on steel reinforcement |
No corrosion |
||
|
9 |
40 Compressive strength/MPa |
1d |
3d |
28d |
|
≥15 |
≥30 |
≥45 |
||
|
10 |
60 Compressive strength/MPa |
1d |
3d |
28d |
|
≥20 |
≥40 |
≥60 |
||
|
11 |
80 Compressive strength/MPa |
1d |
3d |
28d |
|
≥35 |
≥60 |
≥80 |
||
APPLICATION PROCEDURE
· Clean the surface of the foundation, ensuring no debris such as gravel or dust. Before grouting, the foundation surface should be kept moist, without standing water.
· On-site, determine the water-cement ratio based on the recommended ratio. Water temperature between 5-40°C is suitable, and mechanical or manual mixing can be used. Mechanical mixing should be done for 1-2 minutes. For manual mixing, first add 2/3 of the water and mix for 3 minutes, then add the remaining water and continue mixing until uniform.
· The grout should be poured from one side, not from all sides simultaneously. Grouting should be continuous without interruption, and efforts should be made to shorten the grouting time.
· After grouting is completed, any excess material that needs to be removed should be handled before the grout sets.
· After construction, immediately cover with plastic film and add grass curtains or blankets for moisture retention and curing.
TECNICAL INFOMATION
|
Product Technical Parameters |
Packing Specification |
25kg/bag |
|
Character |
Grey mortar |
|
|
Mixing ratio |
Powder: Water = 1:0.12-0.13 (by weight) |
|
|
Shelf life |
12 months when stored unopened in a cool, dry place. |
|
|
Construction Technical Parameters |
Construction Consumption |
2-3t/m³ |
|
Construction Environment |
Working temperature 5°C~35°C. Outdoor construction should be avoided in high temperature, frost, direct sunlight, or windy rainy weather. When the temperature is below 5°C, insulation measures should be done. |
|
|
Operable Time |
30min |
FEATURES AND BENEFITS
· Early strength, high strength:
Compressive strength(40):1-3 days≥30 MPa, 28 days ≥45 MPa.
Compressive strength(60):1-3 days≥40 MPa, 28 days ≥60 MPa.
Compressive strength(80):1-3 days≥60 MPa, 28 days ≥80 MPa.
· High fluidity: Can fill all gaps in equipment foundations without vibration, meeting connection structure requirements.
· High stability: No shrinkage cracks or other defects after formation.
· Micro-expansion: Ensures tight contact between equipment and foundation after grouting.
· Strong durability: Belongs to inorganic bonding material, with a service life longer than that of basic concrete. Withstands hundreds of fatigue test and shows no significant changes in strength after 50 freeze-thaw cycles. Strength significantly increases after soaking in engine oil for 30 days.
· Secondary grouting for equipment foundations.
· Reinforcement and repair of concrete structures.
· Anchoring of foundation bolts and column base plates.
· Anchoring of reverse construction joints in projects such as subways, tunnels, and underground structures.
· Secondary grouting for fixing connections between steel structures (such as steel rails, frames, and columns) and foundations.
Early strength, high strength
High fluidity, High stability
Micro-expansion
Strong durability